1.Machine:PAlAMRY
2.RPM:2500
3. Line Speed:50m/s
4.HRC:55-60
5.Coolant: Oil with water
6.Grinding allowance:1mm
7.Dressing period: 200
8.Use:
The rough grinding and finish grinding by the same wheel to worked. The grinding allowance is 1m'm so remove 0.9mm with rough grinding(In this process that need high RPM and allowed minor burn on the surface so the more important is effectiveness ) then slow down the RPM to remove 0.1mm with finish grinding(In this process would be clear up the burn marks to reach shinning)